  • Spot Wave Cooling Tower Film Fill
Payment Type: L/C, T/T, Western Union
Min. Order: 1
Basic Info

Model No.:  Spot Wave Cooling Tower

Product Description Model NO.: Spot Wave Cooling Tower Material: PVC or PP or UPVC Dimension: 500*1000mmbr 500*1200mm 500*1550mm 500*1800mm Sheet Thickness: 0.33-0.40 mm, Customerization Trademark: NEWIN Origin: China Cooling Method: Counter Flow Condition: New Sheet Space: 25-30-33 mm Applicable Water Temperature: 75ºC ~ -35ºC Transport Package: 20/40/40hq Container with Loose Packing HS Code: 84195000 Physical and mechanical property 
PVC Plastic sheet(before molding) Physical and mechanical property 
No. Item symbol unit symbol test method
1 density ρ g/cm3 ≤1.55 GB/T 1033
2 Heat the longitudinal shrinkage rate S % ≤3.0  
3 tensile strength lengthways
 
σt MPa ≥42.0 GB/T 13022
crosswise
 
≥38.0
4 elongation at break lengthways
 
εt % ≥60 GB/T 13022
crosswise
 
≥35
5 tear strength lengthways
 
σtr kN/m ≥150 GB/T 1130
crosswise
 
≥160
6 Folded in half Coldness 
Resistance Temperature 
ordinary type tb ºC ≤-22  
Frigostabile type ≤-35
*7 Folded in half Coldness Resistance 
Temperature after hygrothermal aging 
ordinary type tb (W·H) ºC ≤-8  
Frigostabile type ≤-18
*8 oxygen index OI   -- ≥40 GB/T 2406
 
 
PVC Plastic sheet(after molding) Physical and mechanical property 
No. Item symbol unit symbol test method
1 density ρ g/cm3 ≤1.55 GB/T 1033
2 tensile strength lengthways
 
σt MPa ≥42.0 GB/T 13022
crosswise
 
≥38.0
3 tear strength lengthways
 
σtr kN/m ≥150 GB/T 1130
crosswise
 
≥160
4 Folded in half Coldness 
Resistance Temperature
ordinary type tb ºC ≤-8  
Frigostabile type ≤-18
*5 oxygen index OI   -- ≥40 GB/T 2406
 
Cooling tower plastic parts code and standard
GB/T 1033-1986 plastic density and relative density experiment method
GB/T 1040-1992 plastic tensile performance test methods
GB/T 1633-1979 thermoplastic softening point (d) test method
GB/T 1843-1996 plastic cantilever beam impact test method
GB/T 2406-1993 plastic combustion performance test method, oxidation index
GB/T 13022-1991 plastic film tensile performance test methods
GB/T 1190-1991 plastic rectangular tear performance test methods











































































































































 

Contact us if you need more details on PVC Film Fills. We are ready to answer your questions on packaging, logistics, certification or any other aspects about Cooling Tower Fills、Cross Flow Film Media. If these products fail to match your need, please contact us and we would like to provide relevant information.

Product Categories : Counter Flow Square Cooling Tower